Thick-core particleboard is a dense, heavy-duty engineered wood product designed for structural stability. It features a uniform, smooth, and void-free surface that’s ideal for veneering, with strong density and load-bearing capacity. Suitable for heavy-duty furniture, countertops, and quality interior door cores, it’s easy to process and cost-effective, though it’s less moisture-resistant than some alternatives.

立即联系

生产流程

原料制备

– Collect raw materials such as wood logs, sawmill residues, and recycled wood.
– Remove impurities (e.g., metal, stones) and debark the logs.
– Cut the materials into small chips (2-5cm in length) using chippers.

纤维生产g

– Steam the wood chips in a digester at 160-180°C for 20-30 minutes to soften the lignin.
– Grind the softened chips into fine fibers using a defibrator (mechanical or thermal-mechanical process).

纤维干燥

– Dry the fibers in a rotary dryer to reduce moisture content to 8-12%.
– Separate and screen the dried fibers to remove oversize particles.

胶合和添加剂的应用

– Mix the fibers with synthetic resin (mainly urea-formaldehyde resin) at a ratio of 8-12% of fiber weight.
– Add wax emulsion (for water resistance) and curing agents as needed.
– Ensure uniform distribution of adhesives through a blending system.

垫层成型

– Convey the fiber-resin mixture to a forming machine.
– Form a continuous, uniform loose mat with controlled thickness and density.

预处理

– Compress the loose mat in a pre-press machine to reduce volume and improve stability.
– Form a semi-hardened slab for easier handling in subsequent processes.

热压

– Transfer the pre-pressed slab to a multi-layer hot press.
– Apply high temperature (180-220°C) and pressure (2.5-4 MPa) for 3-10 minutes.
– The heat cures the resin, and pressure bonds the fibers into a solid board.

冷却和修剪

– Cool the hot-pressed boards to room temperature using cooling racks or fans.
– Trim the edges to achieve standard dimensions (e.g., 2440×1220mm) with saws.

打磨

– Sand both surfaces of the boards using multi-head sanding machines.
– Achieve smoothness and precise thickness (typically 3-30mm).

质量检查和包装

– Inspect boards for defects (e.g., cracks, uneven density, surface imperfections).
– Grade the qualified boards based on quality standards.
– Stack and package the boards for storage or shipment.