了解有关最新建筑材料的专家见解和行业趋势。

OSB

OSB 即定向刨花板,是传统刨花板的升级换代产品,其机械性能具有方向性、耐久性、防潮性,尺寸稳定性也优于普通刨花板。
立即联系
OSB

说明

OSB is the Oriented Strand Board, which is an upgrade of traditional particleboard products. It offers mechanical properties with directionality, durability, moisture resistance, and dimensional stability that exceed those of ordinary particleboard.

With a small expansion coefficient, no distortion, good stability, uniform material, and nail-holding high performance. These all make it a multi-functional wood panel widely used in furniture, packing, decoration, construction, etc.

立即联系

详细信息

产品名称
ORIENTED STRAND BOARD – OSB
原材料
POPLAR, PINE, HARDWOOD OR MIXED
胶水类型
WBP
厚度
6MM/9MM/12MM/15MM/18MM OR AS REQUEST
宽*长
1220X2440MM, 1250X2500MM OR AS REQUEST
水分
8-12%
申请
FURNITURE, DECORATION, PACKING,CONSTRUCTION ETC
付款条款
30%TT IN ADVANCE AND THE BALANCE AGAINST A COPY OF THE BILL, OR LC AT SIGHT
供应能力
每月 10000 立方米
订购数量
20 英尺集装箱
交货时间
支付首付款后 15-20 天

生产流程

原料制备

- 收集原木、锯木厂废料和回收木材等原材料。
- 去除杂质(如金属、石块),并对原木进行去皮。
- 用切片机将材料切成小片(2-5 厘米长)。

纤维生产g

- 将木屑在 160-180°C 的蒸煮器中蒸煮 20-30 分钟,以软化木质素。
- 使用脱纤器(机械或热机械工艺)将软化的碎屑研磨成细纤维。

纤维干燥

- 用旋转式烘干机烘干纤维,将含水量降至 8-12%。
- 分离和筛选干燥的纤维,去除过大的颗粒。

胶合和添加剂的应用

- 按纤维重量 8-12% 的比例将纤维与合成树脂(主要是脲醛树脂)混合。
- 根据需要添加蜡乳液(用于防水)和固化剂。
- 确保通过混合系统均匀分布粘合剂。

垫层成型

- 将纤维-树脂混合物输送到成型机中。
- 形成厚度和密度可控的连续、均匀的松散垫层。

预处理

- 在预压机中压缩松散的垫子,以减少体积并提高稳定性。
- 形成半硬化板坯,便于后续工序的处理。

热压

- 将预压板坯转移到多层热压机上。
- 高温(180-220°C)加压(2.5-4 兆帕)3-10 分钟。
- 热量使树脂固化,压力将纤维粘合成一块坚固的木板。

冷却和修剪

- 用冷却架或风扇将热压板冷却至室温。
- 用锯子将边缘修整至标准尺寸(如 2440×1220mm)。

打磨

- 使用多头打磨机打磨木板的两个表面。
- 实现平滑和精确的厚度(通常为 3-30mm)。

质量检查和包装

- 检查木板是否有缺陷(如裂缝、密度不均、表面瑕疵等)。
- 根据质量标准对合格的电路板进行评级。
- 堆叠和包装电路板,以便储存或装运。

质量控制和包装

我们有一套坚持不懈的装运前检验制度。订单确认后,检验过程立即开始。原材料的等级和类型、加工方法、检验和包装细节将告知工厂管理层。
立即联系

我们的工厂和证书

我们有一套坚持不懈的装运前检验制度。订单确认后,检验过程立即开始。原材料的等级和类型、加工方法、检验和包装细节将告知工厂管理层。
立即联系

联系我们