Pencil cedar plywood is a commercial plywood with grooved lining. Pencil Cedar Plywood can resist moisture and humidity to a certain extent, but it cannot be called “waterproof”. It can withstand certain moisture and humidity, so commercial plywood is most commonly used to make home and office furniture, as well as interior decoration work, such as paneling, kitchen cabinets, car decoration, packaging, sofa interior, photo frame backrest, baby carrier, and crib decoration embossed panels, etc.
Pencil Cedar Plywood has uniform thickness, good dryness and wetness, and good quality. Each worker controls one process and manages it meticulously. The full-core veneer is combined with special glue to increase the adhesion by 30%. The template does not open the glue and can not be layered. It is used 3-5 times more than the ordinary template. It is good for the environment. At the same time, it has good sound absorption and sound insulation performance. The whole production process is controllable and the quality is stable. The surface of the product meets the requirements for direct use, saving a lot of processing costs.
Detalhes
Processo de produção
RAW MATERIALS STORAGE
We have several warehouses to store all our Raw Materials like Poplar Veneer, Hardwood Veneer, Sapelli/Bintangor/Okoume/Pencil Cedar/Pine Face/Back, etc. Once new raw materials delivered into our warehouses, our workers will inspect all and place different grade ram materials into different warehouses.
RAW MATERIALS PRETREATMENT
Once production started, our workers will pretreat the raw materials including the sides joint, gluing.
VENEERS ASSEMBLE
Our workers will assemble the wood veneers one layer by one layer on the assembly line. Like the 18MM will consist of 11 layers wood veneers.
RAW BOARDS PREPRESS
After Veneer Assemble Process, all the Raw Boards need to be prepressed by Cold Press Machine. So that the Raw Boards can be shaped into Raw Plywood. This process need at least 2 hours.
RAW PYWOOD HOT PRESS
Shaped Raw Plywood will be laminated by Hot Press Machine. This process need at least 1 hour. After Hot Press, the Raw Plywood bonding will be strong.
RAW PYWOOD REPATCHING & PUTTYING
This process is to fill the gap on the surface of raw plywood.
RAW PYWOOD SANDING
Put the Raw Plywood into Sanding Machine. After sanding, the raw plywood surface become smooth, and thickness will be even also.
FACE/BACK VENEER ASSEMBLE
Raw Plywood will be glued firstly. Then workers will place the face/back veneer like Sapelli /Bintangor/Okoume/Pencil Cedar on the both sides of raw plywood.
COLD PRESS
After Face/Back Veneer Assemble Process, plywood will be placed into Cold Press Machine again. So that the Face/Back Veneer will bond with the raw plywood initialy. This process need at least 1 hour.
LAMINATED PYWOOD HOT PRESS
This process need at least 30 minutes. After second Hot Press, Face/Back Veneer will bond with the raw plywood strong.
CUTTING & POLISHING
All plywood will be cut into standard size like1220X2440MM. Then plywood will be polished gain to make the face/back smooth.
INSPECTION & PACKING
Inspect boards for defects (e.g., cracks, uneven density, surface imperfections). Grade the qualified boards based on quality standards. Stack and package the boards for storage or shipment.